Designation:SP-205-60 SP-205-65 SP-205-70 Special purpose:The electrode formation of TC.HIK and high voltage disk capacitor |
| 一、Composition Properties: |
1.silver content:SP-205-60: 60±2%; SP-205-65: 65±2%; SP-205-70: 70±2%; 2.viscosity:1500-2000Kcps(4# spindle; 25℃; 0.3r/min; NDJ-8S; shanghai) 3.fineness:≤10μm 4.line resolution: 150-200μm 5.paste coverage:SP-205-60; 140-160cm²/g; SP-205-65; 120-140cm²/g; SP-205-70; 100-120cm²/g; |
| 二、The fired film Properties |
1.Sheet Resistivity:≤5mΩ/□ 2.Condense Film; metallic colour (microscopy) 3.Solderability: coverage>95%(microscopy;Sn62/Pb36/Ag2; 230℃; rosin flux) 4.Solder Resistance:≥5S(Sn62/Pb36/Ag2; 230℃; rosin flux) 5.Adhesion:90° peel≥2Kgf (2mmX2mm pad; ф0.5mm wire; Sn62/Pb36/Ag2; 230℃; rosin flux) |
| 三、Application Guidelines |
1.Screen Print: 180-250mesh; optimum: 200mesh 2.Drying:150℃/3min 3.Firing: peak temperature and time: 800±20℃/10min; cycle:60min 4.Soldering:Sn63/Pb37, Sn60/Pb40 or Sn62/Pb36/Ag2 temperature:215℃-225℃;dipping:1-2sec:flux: rosin flux 5.Storage :Keep in a cool place away from heater or open flames, minimum shelf-life six months. |
| Al Pastes for PTCR |
Designation: AP-202-55 AP-202-60 Special Purpose: The ohmic contact electrode formation of PTCR. |
| 一、Compostition Properties |
1.Silver Content:AP-202-55; 55±2%; AP-202-60; 60±2% 2.Viscosity:1500-2000Kcps(4# spindle; 25℃; 0.3r/min; NDJ-8S; Shanghai) 3.Fineness:≤10μm 4.Coverage:150-170cm²/g |
| 二、The Fired Film Properties |
1.Sheet Resistivity:≤45mΩ/□ 2.Surface Resistance ≤0.1Ω,gap≥2mm 3.Ohmic Characteristic:equal to In50Ga50 electrode.(RA1-RInGa)/RInGa≤2% 4.Heat Age: 250℃/72hr,PTCR for heating △R/R0≤50%; PTCR for limiting current and for erasing △R/R0≤3% 5.Anti-humid:40℃, 95%RH/72hr, no oxide 6.Electrical Current Age:△R/R0≤50%, V=220v±10%/72hr |
| 三、Application Guidelines |
1.Screen print :180-250mesh. optimum: 200mesh 2.Drying:150℃-200℃/3min 3.Firing: peak temp.and time: 650±10℃/5-8min, cycle: 30-45min 4.Thinner:ethylene glycol monobutyl ether or terpineol 5.Storage: keep in a cool place away from heater or open flames, minimum shelf-life six months. |